Behavior of zirconium fuel cladding under fast pressurization rates, Nuclear Engineering and Design, vol.238, pp.1441-1447, 2008. ,
Fuel cladding behavior under rapid loading conditions, s.l, Journal of Nuclear Materials, vol.469, pp.177-186, 2006. ,
Summary and Interpretation of the CABRI REP-Na Program, Nuclear Technology, pp.230-250, 2007. ,
The Influence of Multiaxial States of Stress on the Hydrogen Embrittlement of Zirconium Alloy Sheet, Metall.Trans, vol.16, pp.675-681, 1985. ,
Mechanical Properties of Unirradiated and Irradiated Zr-1% Nb Cladding. s.l. : U.S. Nuclear Regulatory Commission, 2001. ,
The plane strain tests in the PROMETRA program. 127-142, s.l, Journal of Nuclear Materials, vol.472, 2016. ,
Failure characteristics of cladding tubes under RIA conditions through electromagnetic forming. Toronto : s.n, Transactions, 2007. ,
An Improved Testing Device for Measuring Tangential Expandability of Beryllium Tube, Journal of Nuclear Science and Technology, pp.294-297, 1966. ,
Frecture of zircaloy cladding under simulated power ramp conditions, Journal of nuclear materials, pp.209-224, 1973. ,
Experimental Evaluation of Critical Strain Energy Density for Irradiated Cladding under Simulated RIA, Proceedings of ENS Topfuel, 2001. ,
Numerical simulation of the expansion due to compression test, Fuel Safety Research Specialists' Meeting, 2001. ,
Elastic-Plastic Deformation of a Nuclear Fuel Cladding Specimen under the Internal Pressure of a Polymer Pellet, s.n., 2002. WCCM V Fifth World Congress on Computational Mechanics ,
Varias Effect of External Hydride Layer on Fuel-Cladding Deformation during EDC Testing, s.n., 2003. Proc. of the 17th International Conference on Structural Mechanics in Reactor Technology ,
High Temperature Expansion Due to Compression Test for the Determination of a Cladding Material Failure, Proceedings of the 2007 International LWR Fuel Performance Meeting, 2007. ,
Full field measurements used for assessing industrial issues-Two examples, Procedia IUTAM 4, 2012. ,
Effects of Zr-hydride distribution of irradiated Zircaloy-2 cladding in RIA-simulating pellet-clad mechanical interaction testing. 246-252, s.l, Nuclear Engineering and Technology, vol.50, 2018. ,
Improvements in the design and analysis of the segmented expanding mandrel test, journal of Nuclear Materials, vol.131, pp.99-104, 1985. ,
Fracture of Zircaloy-4 cladding tubes with or without hydride blisters in uniaxial to plane strain conditions with standard and optimized expansion due to compression tests, s.l. : Materials Science and Engineering, 2014. ,
URL : https://hal.archives-ouvertes.fr/hal-00966156
Failure Behavior of the Cladding with Outer Surface Pre-crack in Biaxial Stress Test, Proceedings of WRFPM 2014, pp.14-17, 2014. ,
Improved-EDC tests on the Zircaloy-crack. s.l. : Journal of nuclear science and technology, 2016. ,
, Nuclear fuel behaviour under reactivity-initiated accident (RIA) conditions, 2010.
A model to describe the anisotropic viscoplastic mechanical behavior of fresh and irradiated Zircaloy-4 fuel claddings under RIA loading conditions, Journal of Nuclear Materials, vol.379, pp.60-69, 2008. ,
URL : https://hal.archives-ouvertes.fr/hal-00311854
Extension of parametric calculations of the expansion due to compression test using fem model. s.l. : Water Reactor Fuel Performance Meeting, hengdu, China, 2011. ,
Changes to near-surface region of PTFE during dry sliding against steel. s.l, Journal of materials sciences, pp.1877-1885, 1980. ,
The issue of stress state during mechanical tests to assess cladding performance during a reactivity-initiated accident (RIA). 250-267, s.l, Journal of Nuclear Materials, vol.412, 2011. ,